耐腐蚀 PSU/美国苏威/P-1700 WH7407
比重 | ASTM D792 | 1.24 | g/cm³ |
收缩率 流动 2.00mm | ASTM D995 | 0.7 | % |
吸水率 23°C 24hr | ASTM D570 | 0.3 | % |
熔融指数 343°C 2.16kg | ASTM D1238 | 6.5 | g/10min |
拉伸模量 23°C | ASTM D638 | 2480 | MPa |
拉伸强度 23°C | ASTM D638 | 70.3 | MPa |
伸长率 23°C | ASTM D638 | 75 | % |
弯曲强度 23°C | ASTM D790 | 106 | MPa |
弯曲模量 23°C | ASTM D790 | 2690 | MPa |
悬臂梁缺口冲击 23°C | ASTM D256 | 69 | J/m |
热变形温度 未退火 1.80MPa | ASTM D648 | 174 | °C |
体积电阻 | ASTM D257 | 3E16 | Ω.cm |
绝缘强度 | ASTM D149 | 17 | KV/mm |
介电常数 1KHz | ASTM D150 | 3.03 | |
介电常数 1MHz | ASTM D150 | 3.02 | |
耗散因数 1KHz | ASTM D150 | 0.0007 | |
耗散因数 1MHz | ASTM D150 | 0.006 |
防火等级 全色 1.50mm | UL94 | HB | |
防火等级 全色 3.00mm | UL94 | HB | |
防火等级 本色 4.50mm | UL94 | V-0 | |
防火等级 本色 6.00mm | UL94 | V-0 | |
灼热丝起燃温度 0.80mm | IEC 60695 | 875 | °C |
灼热丝起燃温度 1.50mm | IEC 60695 | 850 | °C |
灼热丝起燃温度 3.00mm | IEC 60695 | 850 | °C |
灼热丝起燃温度 6.00mm | IEC 60695 | 850 | °C |
灼热丝相对温度 0.80mm | IEC 60695 | 850 | °C |
灼热丝相对温度 1.50mm | IEC 60695 | 960 | °C |
灼热丝相对温度 3.00mm | IEC 60695 | 960 | °C |
灼热丝相对温度 6.00mm | IEC 60695 | 960 | °C |