高流动 PPS 日本东丽 A503 V0阻燃
A503 物性表
吸水率 | 0.02 | % | ASTM D-570 |
成形收缩率 | 东丽法 | ||
0.25 | % | ||
0.80 | % | ||
流动长 (320℃,98MPa,1mm厚) | 180 | ×10-3m | 东丽法 |
比重 | 1.55 | ASTM D-792 |
摩擦系数 (对钢) | 0.22 | ASTM D-1894 | |
断裂强度 | 75 | ASTM D-732 | |
拉伸强度 | 2.2 | % | ASTM D-638 |
硬度 | 120 | 洛氏 | ASTM D-785 |
摩耗 | 45 | mg/1000回 | ASTM D-1044 |
冲击强度 | ASTM D-256 | ||
130 | J/m | ||
30 | kj/m | ||
弯曲强度 | 205 | MPa | ASTM D-790 |
弯曲弹性体 | 10.0 | GPa | ASTM D-790 |
限界PV值 | 900 | kj/m.hr | 东丽法 |
引张强度 | 155 | MPa | ASTM D-638 |
诱电率 (106Hz) | 3.8 | ASTM D-150 | |
诱电正接 (106Hz) | 0.002 | ASTM D-150 | |
耐电弧性W电级 | 127 | 秒 | ASTM D-495 |
绝缘破坏电压 | 15 | MV/m | ASTM D-149 |
体积固有抵抗 | 10 | Ω.m | ASTM D-257 |
热变形温度 (1.82MPa) | >260 | ℃ | ASTM D-648 |
线膨张系数 | ASTM D-696 | ||
2.9 | ×10-5/K | ||
3.4 | ×10-5/K | ||
燃烧性 | V-0 | UL-94 | |
融点 | 278 | ℃ | DSC |
展开全文