全国服务热线 13532886152

NORYLN225X 沙伯基础PPON225X

更新时间:2024-12-20 07:00:00
价格:请来电询价
品牌:沙伯基础
型号:N225X
性能:尺寸稳定性良好 水解稳定
联系电话:
联系手机: 13532886152
联系人:汪修建
让卖家联系我
详细介绍

PPO 沙伯基础PPON225X

物性信息:

物理性能额定值 (公制)额定值 (英制)

测试方

比重1.11 g/cc1.11 g/ccASTM D792
线性成型收缩率,Flow0.0050 - 0.0070 cm/cm

@Thickness 3.20 mm

0.0050 - 0.0070 in/in

@Thickness 0.126 in

SABIC Method
线性成型收缩率,横向0.0050 - 0.0070 cm/cm

@Thickness 3.20 mm

0.0050 - 0.0070 in/in

@Thickness 0.126 in

SABIC Method
机械性能额定值 (公制)额定值 (英制)测试方法
抗张强度(断裂)49.0 MPa7110 psiType I, 50 mm/min; ASTM D638
抗张强度(屈服)66.0 MPa9570 psiType I, 50 mm/min; ASTM D638
伸长率 (断裂)17 %17 %Type I, 50 mm/min; ASTM D638
屈服伸长率8.0 %8.0 %Type I, 50 mm/min; ASTM D638
弯曲强度99.0 MPa14400 psi2.6 mm/min, 100 mm span; ASTM D790
弯曲模量2.49 GPa361 ksi2.6 mm/min, 100 mm span; ASTM D790
悬壁梁缺口冲击强度1.86 J/cm3.48 ft-lb/inASTM D256

0.960 J/cm

@Temperature -30.0 °C

1.80 ft-lb/in

@Temperature -22.0 °F

ASTM D256

8.86 J/cm

@Thickness 3.20 mm

16.6 ft-lb/in

@Thickness 0.126 in

ASTM D256
落锤总能量39.0 J28.8 ft-lbInstrumented Impact Energy @ peak; ASTM D3763

11.0 J

@Temperature -30.0 °C

8.11 ft-lb

@Temperature -22.0 °F

Instrumented Impact Energy @ peak; ASTM D3763
电气性能额定值 (公制)额定值 (英制)测试方法
体积电阻率2.80e+16 ohm-cm2.80e+16 ohm-cmASTM D257
表面电阻>= 1.00e+14 ohm>= 1.00e+14 ohmASTM D257
介电常数2.55

@Frequency 1.00e+6 Hz

2.55

@Frequency 1.00e+6 Hz

ASTM D150

2.69

@Frequency 50.0 - 60.0 Hz

2.69

@Frequency 50.0 - 60.0 Hz

ASTM D150
介电强度16.2 kV/mm

@Thickness 3.20 mm

411 kV/in

@Thickness 0.126 in

in oil; ASTM D149
耗散因数0.0070

@Frequency 1.00e+6 Hz

0.0070

@Frequency 1.00e+6 Hz

ASTM D150

0.010

@Frequency 50.0 - 60.0 Hz

0.010

@Frequency 50.0 - 60.0 Hz

ASTM D150
耐电弧性60 - 120 sec60 - 120 secTungsten; ASTM D495
相比耐漏电起痕指数(CTI)400 - 600 V400 - 600 VUL 746A
热丝引燃 (HWI)60 - 120 sec60 - 120 secUL 746A
高电弧燃烧,HAI>= 120 arcs>= 120 arcsUL 746A
高压电弧跟踪率,HVTR



联系方式

  • 地址:深圳市龙岗区龙城街道盛平村委田段心南十二巷2号101
  • 联系电话:未提供
  • 销售经理:汪修建
  • 手机:13532886152
  • 微信:13532886152
  • QQ:3137582858
  • Email:3137582858@qq.com